Properties and test methods | Unit | Typical value | Standardization |
Specific surface area (BET) | m2/g | 110 ± 20 | GB/T20020 |
pH value (in 4% dispersion) |
3.8 ~ 5.0 | GB/T20020 | |
Loss on drying (2 hours at 105 °C) |
Wt% | ≤ 0.5 | GB/T20020 |
Loss on ignition (2 hours at 1000 °C, based on material dried for 2 hours at 105 °C) |
Wt% |
≤ 2.0 |
GB/T20020 |
Silica content (based on ignited material) |
Wt% | ≥ 99.8 | GB/T20020 |
Tamped density (based on material dried for 2 hours at 105 °C) |
g/L | 40 ~ 60 | GB/T20020 |
Carbon content (based on material dried for 2 hours at 105 °C) |
Wt% | 0.6 ~ 1.2 | GB/T20020 |