Properties and test methods | Unit | Typical Value | Standardization |
Specific surface area (BET) | m2/g | 260±30 | GB/T20020 |
pH value (in 4% dispersion) |
5.5 ~ 7.8 | GB/T20020 | |
Loss on drying (2 hours at 105 °C) |
Wt% | ≤ 0.5 | GB/T20020 |
Loss on ignition (2 hours at 1000 °C, based on material dried for 2 hours at 105 °C) |
Wt% |
≤ 4.0 |
GB/T20020 |
Silica content (based on ignited material) |
Wt% | ≥ 99.8 | GB/T20020 |
Tamped density (based on material dried for 2 hours at 105 °C) |
g/L | 40 ~ 60 | GB/T20020 |
Carbon content (based on material dried for 2 hours at 105 °C) |
Wt% | 2.8 ~ 4.0 | GB/T20020 |